Metallic glass foil. Amorphous alloy foil. Ribbon: 35 cm x 2,5 cm x 0.0035 cm
$ 12.66
- Description
- Size Guide
Description
cobalt - 83.7%silicon - 9.4%
iron - 3.7%
chrome - 3.2%
magnetic characteristics
Magnetic induction amplitude:
B=0.36 T (
With the amplitude of the magnetic field strength
H=5 A/m)
Magnetic induction amplitude:
B=0.38 T (
With the amplitude of the magnetic field strength
H=25 A/m)
Coercive force: H=0.41 A/m
(
With the amplitude of the magnetic field strength
H=5 A/m)
Relative magnetic permeability:
μ=188'000
(
With the amplitude of the magnetic field strength
H=0.1 A/m)
Material is supplied with heat treatment